Fe 500 and Fe 500D both have a minimum 0.2% proof stress of 500 N/mm², and Fe 550D has 550 N/mm². The "D" grades must meet stricter ductility and chemistry limits: Fe 500D needs 16% minimum elongation against 12% for Fe 500 (IS 1786:2008, Amendment 3 (opens in a new tab)). Your structural engineer specifies which grade a job uses.

Key facts

What do "Fe 500" and the letter "D" mean?

IS 1786 covers deformed steel bars and wires used to reinforce concrete. As amended in 2017, it lists the grades Fe 415, Fe 415D, Fe 415S, Fe 500, Fe 500D, Fe 500S, Fe 550, Fe 550D, Fe 600, Fe 650 and Fe 700 (Amendment 3 (opens in a new tab)).

"Fe" is the chemical symbol for iron. The number is the minimum stress the bar must reach before it yields, measured as 0.2% proof stress, in N/mm². A "D" bar has the same minimum strength as the plain grade, but it must pass extra or tougher tests. In practice, these cover elongation, the ratio of tensile strength to yield strength, and chemical composition.

"TMT" (thermo-mechanical treatment) names the production process, not a grade. The standard's informative Annex A describes it: bars leaving the last rolling stand are partly quenched in water, and the heat left in the core then tempers the hard outer layer (IS 1786:2008, Annex A (opens in a new tab)). The standard leaves manufacturers free to choose any process, as long as the bars meet the required properties.

How do the mechanical properties compare?

These are the minimum values in Table 3 of IS 1786:2008 as replaced by Amendment 3 (March 2017 (opens in a new tab)). The bend-test row comes from Table 4 of the same amendment.

Property (IS 1786 Table 3)Fe 500Fe 500DFe 550D
0.2% proof stress / yield stress, minimum500 N/mm²500 N/mm²550 N/mm²
Tensile strength / yield stress ratio, minimum1.081.101.08
Tensile strength, minimum (absolute)545 N/mm²565 N/mm²600 N/mm²
Elongation, minimum (gauge length 5.65√A)12.0%16.0%14.5%
Total elongation at maximum force, minimumnot specified5%5%
Bend test mandrel, bars up to 20 mm4 × bar size3 × bar size4 × bar size

Three notes on reading the table:

  • The tensile-to-yield ratio is worked out from the actual yield of the test piece. A bar must meet both the ratio and the absolute minimum tensile strength.
  • The standard says the test for total elongation at maximum force is carried out wherever the purchaser specifies it. If your engineer needs that value, put it in your order.
  • A smaller mandrel means a tighter bend. The D grades must bend around a smaller diameter without cracking.

What are the chemical limits?

Clause 4.2, as replaced by Amendment 3, sets maximum percentages in the ladle analysis (Amendment 3 (opens in a new tab)).

Constituent, maximum %Fe 500Fe 500DFe 550D
Carbon0.300.250.25
Sulphur0.0550.0400.040
Phosphorus0.0550.0400.040
Sulphur + phosphorus0.1050.0750.075
Carbon equivalentnot specified0.500.61

The amendment gives the carbon equivalent formula as CE = C + Mn/6 + (Cr + Mo + V)/5 + (Ni + Cu)/15. Lower sulphur and phosphorus limits are one reason a D grade is a different product from the plain grade, even though both share the same strength number.

Why do elongation and the strength ratio matter?

Elongation is how far a test piece stretches before it breaks, as a percentage of its gauge length. Total elongation at maximum force is the stretch at the point where the bar carries its highest load (IS 1786:2008, clauses 3.3 and 3.9 (opens in a new tab)). A higher tensile-to-yield ratio means the bar has a larger strength margin between first yielding and its peak load.

These properties describe ductility: how much a bar can deform before it fails. How much ductility a building, bridge or slab needs is a design question, and the standard does not answer it for a particular site.

So which grade should you buy?

Buy the grade written on the structural drawings or in the bill of quantities. Your structural engineer specifies the grade. It depends on the design code, the loads and the location, and none of that can be settled in a buying guide.

As a buyer, you can:

  • Copy the exact grade, for example "Fe 500D to IS 1786", into your purchase order and your requirement.
  • Ask your engineer before you accept a different grade, even one with a higher number. Fe 550D is not a drop-in swap for Fe 500D: its minimum elongation is lower and its carbon-equivalent limit is higher.
  • List the bar sizes and the quantity per size, and ask for the mill test certificate with each delivery.

For the wider buying process, see our TMT bar buying guide.

How do you check that bars are the grade you ordered?

IS 1786:2008 is on BIS's Scheme-I list, so bars sold under it need a BIS licence and the ISI mark (BIS Scheme-I list (opens in a new tab)). You can read how to check a licence in our guide to checking a BIS licence or CRS registration. For which products need the ISI mark in general, see which products need BIS certification.

The BIS product manual for IS 1786 adds these points (PM/IS 1786/4, July 2020 (opens in a new tab)):

  • Bars must be marked at intervals of no more than 3 metres with the brand name or trade mark, the grade and a six-digit identification number. Two digits identify the BIS branch and four come from the licence number.
  • Each consignment of certified bars must come with a test certificate. It shows the Standard Mark, cast or lot number, grade, size and test results.

The standard also requires a tag on each bundle giving the cast or lot number, the grade and the size (IS 1786:2008, clause 13.2 (opens in a new tab)). Compare the certificate values with the tables above.

Which edition of IS 1786 is this article based on?

This article uses IS 1786:2008 (fourth revision) with Amendments 1 to 4, issued in 2012, 2013, 2017 and 2019 (public copy (opens in a new tab)). BIS's Scheme-I list still names IS 1786:2008 (BIS (opens in a new tab)), and so does the product manual cited above.

However, a newspaper report says BIS's Nagpur office held a workshop on "IS 1786:2025" in July 2026 (The Hitavada, 18 July 2026 (opens in a new tab)). We could not read a 2025 edition or confirm when it takes effect, so some values may have changed. Ask your supplier which edition their test certificate refers to.

How Indibaba can help

You can post a requirement for TMT bars with the exact grade, sizes, quantity per size, delivery city and the documents you need, such as the test certificate. If you only want quotes from checked suppliers, tick "Only verified suppliers (you may get fewer quotes)". You can also see the TMT bars and steel and metals categories; we are still adding suppliers, so some pages have no listings yet.

The values above are the minimums in the standard, not design guidance. Your structural engineer specifies the grade for your structure.

Rules as of 16 November 2026. This article explains public rules in plain English. For a decision about your business, check the official notification or ask your CA.

Frequently asked questions

What is the difference between Fe 500 and Fe 500D?

Both have the same minimum 0.2% proof stress of 500 N/mm² under IS 1786. Fe 500D must also meet stricter requirements: at least 16% elongation instead of 12%, a higher tensile-to-yield ratio (1.10 instead of 1.08), and lower limits on carbon, sulphur and phosphorus.

Is Fe 550D stronger than Fe 500D?

Fe 550D has a higher minimum proof stress (550 N/mm² against 500 N/mm²) and a higher minimum tensile strength (600 N/mm² against 565 N/mm²). Its minimum elongation is lower, at 14.5% against 16%. Which grade suits a structure is decided by the structural engineer.

Which TMT grade is best for house construction?

There is no single answer. The grade is part of the structural design, so your structural engineer specifies it on the drawings, and you should buy exactly that grade.

How do I check the grade of a TMT bar?

BIS-certified bars carry the grade, the brand and a licence-based identification number rolled or marked along the bar. Each consignment should also come with a test certificate showing the grade, cast or lot number and test results.